← Resin Library

TPO

ElastomerAmorphousHygroscopicity NoneField Estimate
Estimate a TPO defect cause from a photo

Drying Conditions

Non-hygroscopic, pre-drying is generally not required.

Melt Temperature

200~230°C

Mold Temperature

15~60°C

Shrinkage

No data

Common Defects & First Checks

Warpage

TPO: thermoplastic olefin, automotive bumper/trim, good impact at low temp.

View Guide
Sink Mark

TPO: thermoplastic olefin, automotive bumper/trim, good impact at low temp.

View Guide

Field Notes

TPO: thermoplastic olefin, automotive bumper/trim, good impact at low temp.

Got a defect with TPO? Upload a photo and settings, we'll estimate the cause

Related Resins

Keep using it on the floor. Your estimate history and machine conditions build up in the app.

5 free estimates when you sign up

This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.