← Resin Library

PA/ABS

BlendAmorphousHygroscopicity ModerateField Estimate
Estimate a PA/ABS defect cause from a photo

Drying Conditions

Temperature
80°C
Time
4h
Target Moisture
N/A

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

240~270°C

Mold Temperature

40~80°C

Shrinkage

No data

Common Defects & First Checks

Silver Streak

PA/ABS: two-phase blend, impact-modified PA.

View Guide

Field Notes

PA/ABS: two-phase blend, impact-modified PA. PA phase is hygroscopic → drying critical.

Got a defect with PA/ABS? Upload a photo and settings, we'll estimate the cause

Related Resins

Keep using it on the floor. Your estimate history and machine conditions build up in the app.

5 free estimates when you sign up

This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.