← Resin Library

PBT/ABS

BlendAmorphousHygroscopicity ModerateField Estimate
Estimate a PBT/ABS defect cause from a photo

Drying Conditions

Temperature
120°C
Time
3h
Target Moisture
N/A

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

240~270°C

Mold Temperature

60~80°C

Shrinkage

No data

Common Defects & First Checks

Sink Mark

PBT/ABS: good surface quality, chemical resistance.

View Guide
Weld Line

PBT/ABS: good surface quality, chemical resistance.

View Guide

Field Notes

PBT/ABS: good surface quality, chemical resistance. Process at lower end to avoid ABS degradation.

Got a defect with PBT/ABS? Upload a photo and settings, we'll estimate the cause