PE(HDPE)

CommodityCrystallineHygroscopicity NoneVerified
Estimate a PE(HDPE) defect cause from a photo

Drying Conditions

Non-hygroscopic, pre-drying is generally not required.

Melt Temperature

200~250°C

Mold Temperature

20~50°C

Shrinkage

1.5~3%

Common Defects & First Checks

Warpage

HDPE: commodity, high shrinkage 1.

View Guide
Sink Mark

HDPE: commodity, high shrinkage 1.

View Guide

Field Notes

HDPE: commodity, high shrinkage 1.5-3.0%. Similar to PP but lower stiffness. Warpage and sink mark.