← Resin Library
PA6T
Super-EngineeringCrystallineHygroscopicity ModerateField Estimate
Estimate a PA6T defect cause from a photo Drying Conditions
Temperature
120°C
Time
4-6h
Target Moisture
N/A
A dehumidifying dryer is recommended (relatively hygroscopic).
Melt Temperature
320~340°C
Mold Temperature
130~150°C
Shrinkage
No data
Common Defects & First Checks
Flash
PA6T(PPA): semi-aromatic, high heat resistance.
Burn Mark
PA6T(PPA): semi-aromatic, high heat resistance.
Short Shot
PA6T(PPA): semi-aromatic, high heat resistance.
Field Notes
PA6T(PPA): semi-aromatic, high heat resistance. High fluidity → flash. High-temp processing → burn risk. Fast solidification → short shot.
Related Resins
Keep using it on the floor. Your estimate history and machine conditions build up in the app.
5 free estimates when you sign up
This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.