PAI
Super-EngineeringAmorphousHygroscopicity HighField Estimate
Estimate a PAI defect cause from a photo Drying Conditions
Temperature
120°C
Time
16h
Target Moisture
N/A
A dehumidifying dryer is recommended (relatively hygroscopic).
Melt Temperature
330~370°C
Mold Temperature
200~230°C
Shrinkage
No data
Common Defects & First Checks
No notable defect tendency recorded in the KB.
Field Notes
PAI: highest performance thermoplastic, requires post-cure and special equipment/expertise. Drying 16hrs minimum.
Related Resins
Keep using it on the floor. Your estimate history and machine conditions build up in the app.
5 free estimates when you sign up
This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.