← Resin Library

PEI

Super-EngineeringAmorphousHygroscopicity ModerateField Estimate
Estimate a PEI defect cause from a photo

Drying Conditions

Temperature
150°C
Time
4-6h
Target Moisture
0.02%

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

350~400°C

Mold Temperature

135~175°C

Shrinkage

No data

Common Defects & First Checks

Short Shot

PEI: very high melt viscosity → needs high injection pressure → short shot risk.

View Guide
Silver Streak

PEI: very high melt viscosity → needs high injection pressure → short shot risk.

View Guide

Field Notes

PEI: very high melt viscosity → needs high injection pressure → short shot risk. Moisture → splay. Beyond 9-type: stress cracking. Transparent amber.

Got a defect with PEI? Upload a photo and settings, we'll estimate the cause

Related Resins

Keep using it on the floor. Your estimate history and machine conditions build up in the app.

5 free estimates when you sign up

This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.

JINSIMLABS.COM