← Resin Library
PPSU
Super-EngineeringAmorphousHygroscopicity ModerateField Estimate
Estimate a PPSU defect cause from a photo Drying Conditions
Temperature
150°C
Time
4h
Target Moisture
N/A
A dehumidifying dryer is recommended (relatively hygroscopic).
Melt Temperature
350~390°C
Mold Temperature
140~180°C
Shrinkage
No data
Common Defects & First Checks
Silver Streak
PPSU: sterilizable (medical applications), better hydrolytic stability than PSU.
Field Notes
PPSU: sterilizable (medical applications), better hydrolytic stability than PSU.