PSU

Super-EngineeringAmorphousHygroscopicity ModerateField Estimate
Estimate a PSU defect cause from a photo

Drying Conditions

Temperature
140°C
Time
4h
Target Moisture
N/A

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

330~380°C

Mold Temperature

120~160°C

Shrinkage

No data

Common Defects & First Checks

Silver Streak

PSU(Polysulfone): transparent, chemical resistance but sensitive to certain solvents.

View Guide

Field Notes

PSU(Polysulfone): transparent, chemical resistance but sensitive to certain solvents. Moisture → splay. Beyond 9-type: stress cracking.