EngineeringCrystallineHygroscopicity HighField Estimate
Estimate a PA6/66 defect cause from a photo Drying Conditions
Temperature
80°C
Time
4-6h
Target Moisture
N/A
A dehumidifying dryer is recommended (relatively hygroscopic).
Melt Temperature
240~270°C
Mold Temperature
60~90°C
Shrinkage
No data
Common Defects & First Checks
Silver Streak
PA6/66 copolymer: intermediate between PA6 and PA66, broader processing window than PA66.
Sink Mark
PA6/66 copolymer: intermediate between PA6 and PA66, broader processing window than PA66.
Warpage
PA6/66 copolymer: intermediate between PA6 and PA66, broader processing window than PA66.
Field Notes
PA6/66 copolymer: intermediate between PA6 and PA66, broader processing window than PA66. Still hygroscopic — check drying.
Related Resins
Keep using it on the floor. Your estimate history and machine conditions build up in the app.
5 free estimates when you sign up
This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.