EngineeringCrystallineHygroscopicity ModerateField Estimate
Estimate a PA610 defect cause from a photo

Drying Conditions

Temperature
80°C
Time
3-4h
Target Moisture
0.1%

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

240~270°C

Mold Temperature

40~90°C

Shrinkage

No data

Common Defects & First Checks

Silver Streak

PA610: less hygroscopic than PA6/66, good balance of properties, similar processing approach.

View Guide
Sink Mark

PA610: less hygroscopic than PA6/66, good balance of properties, similar processing approach.

View Guide

Field Notes

PA610: less hygroscopic than PA6/66, good balance of properties, similar processing approach.

Got a defect with PA610? Upload a photo and settings, we'll estimate the cause

Related Resins

Keep using it on the floor. Your estimate history and machine conditions build up in the app.

5 free estimates when you sign up

This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.

JINSIMLABS.COM