← Resin Library

PCT

EngineeringCrystallineHygroscopicity ModerateField Estimate
Estimate a PCT defect cause from a photo

Drying Conditions

Temperature
120°C
Time
4h
Target Moisture
N/A

A dehumidifying dryer is recommended (relatively hygroscopic).

Melt Temperature

280~310°C

Mold Temperature

100~130°C

Shrinkage

No data

Common Defects & First Checks

Warpage

PCT: higher heat resistance than PBT/PET, similar to PBT but higher processing temperatures.

View Guide
Sink Mark

PCT: higher heat resistance than PBT/PET, similar to PBT but higher processing temperatures.

View Guide

Field Notes

PCT: higher heat resistance than PBT/PET, similar to PBT but higher processing temperatures.

Got a defect with PCT? Upload a photo and settings, we'll estimate the cause

Related Resins

Keep using it on the floor. Your estimate history and machine conditions build up in the app.

5 free estimates when you sign up

This data is a field-reference summary. Always verify against the resin manufacturer’s official TDS.

JINSIMLABS.COM