Void/Bubble

Internal voids inside the part that may not be visible from the surface.

Estimate your void/bubble cause from a photo

◆ Common Causes

  • •Insufficient hold pressure
  • •Insufficient hold time
  • •Premature gate freeze
  • •Injection speed too high
  • •Inadequate resin drying

◆ Solutions

  • ✓Increase hold pressure
  • ✓Increase hold time
  • ✓Enlarge gate size
  • ✓Reduce injection speed (final stage)
  • ✓Verify resin drying

◆ Resin-Specific Notes

PC

Voids easily form in thick sections.

PA

Moisture-induced bubbles. Drying mandatory.

Transparent

Voids are visible in transparent resins. Strict control required.